725

UNS #N07725

725 alloy is a precipitation hardenable, nickel-base alloy that offers exceptional resistance to stress corrosion cracking and general pitting and crevice corrosion in the age hardened condition. With corrosion resistance similar to 625 and superior to that of 718, 725 is considered for applications where severely corrosive environments are a concern. A yield strength (0.2% offset) above 120 ksi (827 MPa) can be obtained by aging without prior warm or cold working. The precipitation hardening capability is particularly important in applications where large-section size or intricate shape precludes warm working.

Type Analysis

  • Carbon (Maximum) 0.03
  • Phosphorus (Maximum) 0.015
  • Silicon (Maximum) 0.2
  • Nickel (Maximum) 59
  • Titanium (Nominal) 1.6
  • Manganese (Maximum) 0.2
  • Sulfur (Maximum) 0.01
  • Chromium (Nominal) 22
  • Cobalt (Nominal) 4
  • Molybdenum (Nominal) 9.5
  • Iron (Nominal) Balance
  • Aluminum (Nominal) 0.35

Applications

Applicable Specifications

  • ASTM B805
  • NACE MR0175

RELATED RESOURCES

Browse our growing library of resources including case studies, product brochures, technical data sheets, product selection guides and more.