ACUBE® 100

ACUBE 100 alloy is a non-magnetic, cobalt-base alloy exhibiting high strength, excellent corrosion resistance, and outstanding wear resistance. ACUBE 100 is beryllium free and can be considered as a replacement for copper-beryllium alloys, eliminating the health and safety issues associated with beryllium-containing alloys as beryllium dust has been tied to a variety of health hazards. Can be considered for applications that required superior resistance to galling and wear. A premium-melted alloy, finished mill ACUBE 100 can be supplied in the annealed, hot worked, or work strengthened (warm worked) condition.

Type Analysis

  • Carbon (Maximum) 0.15
  • Silicon (Maximum) 1
  • Nickel (Nominal) 1
  • Manganese (Maximum) 1
  • Chromium (Nominal) 26.00 - 30.00
  • Cobalt (Nominal) Balance
  • Molybdenum (Nominal) 5.00 - 7.00
  • Iron (Nominal) 1
  • Nitrogen (Nominal) 0.25

Applicable Specifications

  • AMS 5918

Bar

Rounds

Billet

Wire

Rod

RELATED RESOURCES

Browse our growing library of resources including case studies, product brochures, technical data sheets, product selection guides and more.