Type Analysis

  • Carbon (Nominal) 0.33
  • Silicon (Maximum) 12
  • Chromium (Nominal) 2.25
  • Cobalt (Nominal) 15.6
  • Molybdenum (Nominal) 1.85
  • Iron (Nominal) Balance