AerMet® 100

UNS #K92580

AerMet® 100 an alloy providing high hardness and strength combined with exceptional ductility and toughness. The alloy is designed for components requiring high strength, high fracture toughness and exceptional resistance to stress corrosion cracking and fatigue.

Type Analysis

  • Carbon (Nominal) 0.23
  • Nickel (Nominal) 11.5
  • Chromium (Nominal) 3.1
  • Cobalt (Nominal) 13.5
  • Molybdenum (Nominal) 1.2
  • Iron (Nominal) Balance

Applicable Specifications

  • AMS 6478
  • AMS 6532
  • McDonnell Douglas MMS 217
  • MIL HDBK-5

Bar

Hollow Bar

Rounds

Billet

Plate

Strip

Sheet

Wire

Weld Wire