Conichrome®

UNS #R30008 & R30003

Conichrome® is a non-magnetic, austenitic Nickel-Cobalt-Chromium-Molybdenum alloy possessing a unique combination of extremely high strength, ductility, excellent corrosion resistance, and high fatigue strength. Manufactured using premium melting and remelting operations, the alloy has extremely good cleanliness (low inclusion content) and improved homogeniety, which are vital to the performance, properties, and functionality of this alloy in its demanding applications.

Type Analysis

  • Carbon (Maximum) 0.15
  • Phosphorus (Maximum) 0.015
  • Silicon (Maximum) 1.2
  • Nickel (Nominal) 14.0-18.0
  • Manganese (Maximum) 1.0-2.5
  • Sulfur (Maximum) 0.015
  • Chromium (Nominal) 18.5-21.5
  • Cobalt (Nominal) 39.0-42.0
  • Molybdenum (Nominal) 6.0-8.0
  • Iron (Nominal) Balance

Downloads

Request a Quote

Applicable Specifications

  • ASTM 1058
  • NACE MR0175
  • ISO5832-7
  • AMS 5833

Bar

Rounds

Strip

Coil

Wire

Rod

RELATED RESOURCES

Browse our growing library of resources including case studies, product brochures, technical data sheets, product selection guides and more.