HyTuf

UNS #K32550

HyTuf is a high strength low alloy steel. In the 220/240 KSI Tensile range, it has good ductility, fracture toughness, and impact strength. The alloy is Vacuum Arc Remelted to optimize cleanliness and preferred ingot structure for superior mechanical properties.

Type Analysis

  • Carbon (Nominal) 0.25
  • Silicon (Nominal) 1.5
  • Nickel (Nominal) 1.8
  • Manganese (Nominal) 1.35
  • Chromium (Nominal) 0.3
  • Molybdenum (Nominal) 0.4
  • Iron (Nominal) Balance

Applications

Aircraft landing gear, flap tracks, and other structural applications

Applicable Specifications

  • AMS 6425
  • MIL S 7108
  • EMS 126
  • DMS 1841
  • NAI 1275

Bar