Low Expansion 45

Low Expansion 45 has a relatively constant rate of thermal expansion to about 800°F (538°C).

Type Analysis

  • Carbon (Maximum) 0.05
  • Silicon (Maximum) 0.25
  • Nickel (Nominal) 45
  • Manganese (Maximum) 0.4
  • Iron (Nominal) Balance

Applications

Thermostats