Temperature Compensator 80

Temperature Compensator 80 is a temperature-compensating alloy having specific permeability versus temperature characteristics.

Type Analysis

  • Nickel (Nominal) Balance
  • Copper (Nominal) 19-22

Applications

Temperature sensing and modulation equipment. Electronics incorporating temperature compensation.