Ti CP Grade 2

UNS #R50400

Ti CP Grade 2 has higher tolerable levels of iron and oxygen and is widely used because it combines excellent formability and moderate strength with superior corrosion resistance. It has a minimum yield strength of 275 Mpa (40 ksi), and relatively low levels of impurity elements, which places it between Grades 1 and 3 in terms of strength.

Type Analysis

  • Carbon (Maximum) 0.08
  • Titanium (Nominal) Balance
  • Iron (Nominal) 0.3
  • Nitrogen (Maximum) 0.03
  • Hydrogen (Maximum) 0.015
  • Oxygen (Maximum) 0.25

Applicable Specifications

  • AMS 4902 (Sheet
  • Strip
  • Plate)
  • AMS 4942 (Seamless Tubing)
  • ASTM B265 (Sheet
  • Strip
  • Plate)
  • ASTM B367 (Castings)
  • AWS A5.16-70 (Weld Filler Metal Wire and Rod)
  • AMS 4941 (Welded Tubing)
  • AMS 4951 (Weld Filler Metal Wire)
  • ASTM B348 (Bar
  • Billet)
  • ASTM F67 (Unalloyed Ti for Surgical Implants)

Bar

Rounds

Shapes

Ultrabar Precision Bar

Ingot

Strip

Sheet

Wire

Dynalube Coil

Shapes

Smart Coil Titanium Coil

Weld Wire

RELATED RESOURCES

Browse our growing library of resources including case studies, product brochures, technical data sheets, product selection guides and more.