15-15HS® Max Stainless

Composition (Nominal)
0.04 C, 16.00/19.00 Mn, 0.050 P, 0.050 S, 1.00 Si, 18.00/21.00 Cr, 3.00 Ni, 0.50/3.00 Mo, 0.50/0.80 N, Bal. Fe

An austenitic, nitrogen-strengthened stainless steel. It can be considered for oil and gas industry applications such as nonmagnetic drill collars, stabilizers, and MWD housings, especially when high strength 140 ksi (966 MPa) minimum yield strength is desired.

A post-machining ID compressive stress treatment for drill collars has been developed to further improve the resistance to stress-corrosion cracking. 15-15HS Max is capable of high strength with improved pitting corrosion resistance when compared with competitive Cr-Mn-N stainless alloys.

PRODUCT RESOURCES

LITERATURE

Carpenter Technology Corporation Carpenter Technology Corporation

Carpenter Technology Corporation (NYSE: CRS) is a recognized leader in high-performance specialty alloy-based materials and process solutions for critical applications in the aerospace, defense, transportation, energy, industrial, medical, and consumer electronics markets.

Learn More »