35NCD16 Alloy

Composition (Nominal):
0.40 C, 0.45 Mn, 0.30 Si, 4.00 Ni, 1.80 Cr, 0.45 Mo, 0.03 V

35NCD16 VAC-ARC is a high strength, low alloy vacuum arc remelted steel that takes its name from the French industry designation. A combination of high strength, high fracture toughness and superior cleanliness makes this alloy a candidate for aerospace structural applications.