405 Stainless

Single Figures are Maxinums
0.08 C, 11.50-14.50 Cr, 1.00 Mn, 1.00 Si, 0.040 P, 0.030 S, 0.10-0.30 Al, Balance Fe

A nonhardenable stainless steel that has been used in the as-welded condition. It has been used for welded applications that require finish machining. Corrosion resistance is similar to that of Type 410. The alloy possesses acceptable resistance to sulfide stress cracking at Rockwell C 22 maximum hardness per NACE MR-01-75.