EnduraMet® 2205 Stainless

UNS S31803 | DIN 1.4462

Composition (Nominal)
C 0.03, Mn 2.00, P 0.030, Sulfur 0.020, Si 1.00, Cr 22.00, Ni 5.50, Mo 3.00,
N 0.20, Fe Balance

EnduraMet 2205 stainless is a duplex stainless steel that has a microstructure consisting of austenite and ferrite phases. This duplex microstructure and the chemical composition of EnduraMet 2205 stainless results in an excellent combination of strength and corrosion resistance.

EnduraMet 2205 stainless has twice the annealed yield strength of typical austenitic stainless steels, like Type 304 and 316. In the hot rolled unannealed condition, yield strength of 75 ksi (518 MPa) or higher can be achieved for bar diameters up to 1.375 in. (34.925mm).

EnduraMet 2205 stainless possesses good resistance to general corrosion in many acid environments and, has excellent resistance to chloride stress corrosion cracking, pitting and crevice corrosion.

Specifications: ASME SA479, ASTM A240, ASTM A276, ASTM A479, ASTM A955M, BS 6744: 2001, NACE MR0175