Composition (Nominal)
C 0.06, Mn 14.00, P 0.060, S 0.030, Si 1.00, Cr 19.00, Ni 2.50, N 0.45, Fe Balance
EnduraMet® 32 stainless is a high-manganese, low-nickel, nitrogen-strengthened austenitic stainless steel. By means of solid solution strengthening, the nitrogen provides significantly higher yield and tensile strength as annealed than conventional austenitic stainless steels such as Type 304 and Type 316, without adversely affecting ductility, corrosion resistance or non-magnetic properties. In the hot rolled unannealed condition, yield strengths of 75 ksi (518 MPa) or higher can be achieved for bar diameters up to 2 in. (50.8 mm).
Specifications: ASTM A276 (Grade XM-28), ASTM A313 (Grade XM-28), ASTM A580 (Grade XM-28), ASTM A955 (Grade XM-28)