CarTech Puris 5+ titanium powder is a custom composition of Ti-6Al-4V that meets all the specifications of Grade 5 while maintaining high strength with low oxygen content.

Typically additive manufacturers seek to balance the oxygen levels needed to obtain the desired strength properties with the increases in oxygen levels inherent in some additive-manufacturing processes.

This creates a challenge in laser melt or e-beam direct melt 3D printing, as both processes experience increases in oxygen content with each recycle of excess powder from the build box. By starting with CarTech Puris 5+ titanium powder, customers can manage this balance of oxygen and strength better throughout the life cycle of the titanium powder.

PRODUCT RESOURCES

LITERATURE

Carpenter Technology Corporation Carpenter Technology Corporation

Carpenter Technology Corporation (NYSE: CRS) is a recognized leader in high-performance specialty alloy-based materials and process solutions for critical applications in the aerospace, defense, transportation, energy, industrial, medical, and consumer electronics markets.

Learn More »