SCF 19® Max Alloy

UNS S21000
Composition (Nominal):
0.03 C, 5.00 Mn, 0.025 P, 0.003 S, 0.40 Si, 20.00 Cr, 18.00 Ni, 5.00 Mo, 0.35 N, Bal. Fe

An austenitic, nitrogen-strengthened stainless steel. Because of its combination of stress-corrosion-cracking resistance, high strength, and low magnetic permeability, it has been used as a nonmagnetic drill collar and MWD housing alloy. Laboratory and field evaluations have shown its superiority over the conventional chromium-manganese stainlesses commonly used for such applications.