Titanium Alloy 15V-3Cr-35N-3Al

(15% vanadium, 3% chrome, 4% tin, 2% aluminum)

Ti 15V-3Cr-3Sn-3Al, a titanium beta alloy, is highly heat-treatable to a wide range
of mechanical properties. It also has excellent cold-formability.