Titanium Alloy Ti-0.2Pd

(0.2% palladium)

Ti-0.2Pd is a commercially pure titanium with modifications. The addition of palladium to commercially pure titanium greatly increases its resistance to crevice corrosion in reducing environments. ASTM B348 Grade 7 and Grade 11 both have 0.2 % palladium, with Grade 7 possessing a higher oxygen and iron content (greater strength but lower ductility) than Grade 11.