Titanium Alloy Ti 3Al-2.5V

(3% aluminum, 2.5% vanadium)

Ti 3Al-2.5V is a titanium near-alpha alloy that represents a good compromise between formability and strength. It is stronger than commercially pure titanium (at both room and elevated temperatures). Unlike Ti 6Al-4V, it has the ability to be cold-rolled. It is also known as ASTM B348 Grade 9.