Titanium Alloy Ti-3Al-8V-6Cr-4Mo-4Zr (Beta C™)

Single figures are nominal except where noted

0.05 C, 3.50/4.50 Mo, 3.00/4.00 Al, 3.50/4.50 Zr, 0.30 Fe, 0.030 H,
5.50/6.50 Cr, Bal. Ti, 7.50/8.50 V, 0.03 N,
0.120 O, 0.005 Y, 0.40 Other/Total

* Other, Each (Maximum) = 0.150%

Ti-3-8-6-4-4 (Beta C) is heat-treatable to a wide range of strength levels, making it appropriate for applications where very high strength, light weight and corrosion resistance are important. It has become a standard material for a particular niche of specialized applications which have included aircraft springs, underground tubes, and casing equipment for gas and oil well operations, due to its low elastic modules and excellent fatigue resistance. It has also been used in fasteners and high-performance auto racing applications. Beta C is also known as ASTM B348 Grade 19.

Specifications: AMS 4957 (Bar, Wire, Cold Drawn), AMS 4958 (Bar, Rod, STA), MIL-T 9046 (Sheet, Strip, Plate), MIL-T 9047 (Bars, Billets)

PRODUCT RESOURCES

LITERATURE

Carpenter Technology Corporation Carpenter Technology Corporation

Carpenter Technology Corporation (NYSE: CRS) is a recognized leader in high-performance specialty alloy-based materials and process solutions for critical applications in the aerospace, defense, transportation, energy, industrial, medical, and consumer electronics markets.

Learn More »