Titanium Alloy Ti Cb

Titanium-Columbium (Niobium) Alloy

Ti-Cb has a nominal composition of 55% titanium and 45% columbium (also known as niobium). Its use is compatible with oxygen-rich environments, and it possesses excellent corrosion resistance, moderate strength levels, and a very low elastic modulus. It is also known as ASTM B348 Grade 36.