17-4 Select™

UNS #S17400

17-4 Select is a martensitic precipitation/age-hardening stainless steel offering high strength and hardness along with excellent corrosion resistance. It has good fabricating characteristics and can be age hardened by a single-step, low temperature treatment with controlled residual stresses.

Type Analysis

  • Carbon (Maximum) 0.07
  • Phosphorus (Maximum) 0.04
  • Silicon (Maximum) 1
  • Nickel (Nominal) 3.00-5.00
  • Manganese (Maximum) 1
  • Sulfur (Maximum) 0.03
  • Chromium (Nominal) 15.00-17.50
  • Cobalt (Nominal) <0.1
  • Iron (Nominal) Balance
  • Copper (Nominal) 3.00-5.00
  • Columbium+Tantalum (Nominal) 0.15-0.45

Downloads

Request a Quote

Applicable Specifications

  • AMS 5643
  • ASTM A564
  • ASME SA564

Bar