AerMet® 310

AerMet® 310 alloy possesses higher hardness and strength than AerMet® 100 alloy while exhibiting exceptional ductility and toughness. At a 310 ksi (2137 MPa) ultimate tensile strength, it exhibits toughness values equivalent to alloys 20 ksi (138 MPa) lower in strength. The alloy should be considered as a candidate for use in components requiring high strength, high fracture toughness and exceptional resistance to stress corrosion cracking and fatigue.

Type Analysis

  • Carbon (Nominal) 0.25
  • Nickel (Nominal) 11
  • Chromium (Nominal) 2.4
  • Cobalt (Nominal) 15
  • Molybdenum (Nominal) 1.4
  • Iron (Nominal) Balance

Applications

Armor, Landing gear, Actuators, Ordnance, Structural tubing, Ballistic tolerant components, Jet engine shafts, Structural members, Drive shafts

Applicable Specifications

Billet

Hollow Bar

Plate

Rounds

Strip

Sheet

Wire