AerMet® for Tooling

UNS #K92580

AerMet® for Tooling is a double-vacuum melted, iron-cobalt-nickel alloy possessing high hardness and strength combined with exceptional ductility and toughness. The alloy is designed for components which require a combination of HRC 53/55 hardness with the highest toughness available.

Type Analysis

  • Carbon (Nominal) 0.23
  • Nickel (Nominal) 11.5
  • Chromium (Nominal) 3.1
  • Cobalt (Nominal) 13.5
  • Molybdenum (Nominal) 1.2
  • Iron (Nominal) Balance

Applications

Punches Blanking dies Crimping dies Embossing dies Shrink rings Test equipment Collets Chuck jaws Shear blades Jigs Fixtures Structural members Coining dies Shafts Mandrels Retaining rings Swaging tools

Applicable Specifications

  • AMS 6478
  • AMS 6532
  • McDonnell Douglas MMS 217
  • MIL HDBK-5

Billet

Hollow Bar

Plate

Rounds

Strip

Sheet

Weld Wire