EnduraMet 32 is a high-manganese, low-nickel, nitrogen-strengthened austenitic stainless steel. By means of solid solution strengthening, the nitrogen provides significantly higher yield and tensile strength as annealed than conventional austenitic stainless steels such as 304 and 316, without adversely affecting ductility, corrosion resistance or non-magnetic properties. In the hot rolled unannealed condition, yield strengths of 75 ksi (518 MPa) or higher can be achieved for bar diameters up to 2 in. (50.8 mm).

Type Analysis

  • Carbon (Maximum) 0.06
  • Phosphorus (Maximum) 0.06
  • Silicon (Maximum) 1
  • Nickel (Nominal) 0.50-2.50
  • Manganese (Maximum) 11.00-14.00
  • Sulfur (Maximum) 0.03
  • Chromium (Nominal) 16.50-19.00
  • Iron (Nominal) Balance
  • Nitrogen (Nominal) 0.20-0.45

Applications

rebar in bridge decks, barrier and retaining walls, anchoring systems, chemical plant infrastructure, coastal piers and wharves, bridge parapets, sidewalks and bridge pilings, dowel bars, welded-wire mesh and tie wire.

Applicable Specifications

  • ASTM A276 (Grade XM-28)
  • ASTM A580 (Grade XM-28)
  • ASTM A313 (Grade XM-28)
  • ASTM A955 (Grade XM-28)