Micro-Melt® T15 Plus

Micro-Melt® T15 Plus is a high alloy content high speed powder metal tool steel with improved hardness capability and wear resistance compared to standard M-series high speed steels.

Type Analysis

  • Carbon (Nominal) 1.6
  • Tungsten (Nominal) 10.5
  • Sulfur (Maximum) 0.03
  • Chromium (Nominal) 4.8
  • Cobalt (Nominal) 8
  • Molybdenum (Nominal) 2
  • Iron (Nominal) Balance
  • Vanadium (Nominal) 5

Applications

Hobs End Mills Broaches Punches Milling Cutters Twist Drills Form Tools Thread Roll Dies Taps Indexable Inserts