CP Ti - Grade 1

UNS #R50250

CP Ti - Grade 1 has the lowest strength and best ductility of the four primary ASTM grades due to its higher level of purity. Commercially pure titanium grades have high corrosion resistance, excellent biocompatibility and good formability. They are classified base on their yield strength and allowable levels of the elements iron, carbon, nitrogen, and oxygen level.

Type Analysis

  • Carbon (Maximum) 0.08
  • Titanium (Nominal) Balance
  • Iron (Nominal) 0.2
  • Nitrogen (Maximum) 0.03
  • Hydrogen (Maximum) 0.012
  • Oxygen (Maximum) 0.18

Downloads

Request a Quote

Applicable Specifications

  • ASTM F67
  • ISO 5832-2