NiMark® T-250

UNS #K92150

NiMark® T-250 is a titanium-strengthened 18% nickel maraging steel designed to achieve ultra-high strength (250 ksi UTS) and toughness of NiMark® 250 (cobalt-strengthened 18% nickel maraging steel). NiMark® T-250 contains no cobalt and less molybdenum than NiMark® 250 to reduce raw material cost without sacrificing mechanical strength or toughness. NiMark® T-250 is vacuum induction melted (VIM) plus vacuum arc remelted (VAR) to achieve a very clean and homogeneous microstructure, which contributes to toughness and fatigue performance. Like other nickel maraging alloys, NiMark® T-250 is typically supplied in the solution annealed condition, and peak properties are developed after a simple one-step, low-temperature aging thermal treatment (900°F, 4–6 hours, air cool). A high degree of dimensional stability is maintained through the aging process.

Type Analysis

  • Carbon (Maximum) 0.030
  • Phosphorus (Maximum) 0.010
  • Silicon (Maximum) 0.10
  • Nickel (Nominal) 18.00-20.00
  • Titanium (Nominal) 1.30-1.45
  • Manganese (Maximum) 0.10
  • Sulfur (Maximum) 0.010
  • Chromium (Maximum) 0.50
  • Molybdenum (Nominal) 2.75-3.25
  • Iron (Nominal) Balance
  • Aluminum (Nominal) 0.05-0.15
  • Copper (Maximum) 0.50
  • Boron (Nominal) 0.003
  • Zirconium (Nominal) 0.020
  • Cobalt (Maximum) 0.50

Downloads

Request a Quote

Applicable Specifications

  • AMS 6519
  • MIL-S-47319A

Bar

Rounds

Billet

RELATED RESOURCES

Browse our growing library of resources including case studies, product brochures, technical data sheets, product selection guides and more.