PowderRange® 625

UNS #N06625

PowderRange® 625 is a non-magnetic, corrosion and oxidation resistant, nickel-base superalloy. Its outstanding strength and toughness in the temperature range cryogenic to 2000°F (1093°C) are derived primarily from the solid solution effects of the refractory metals, niobium and molybdenum, in a nickel-chromium matrix. The alloy has excellent fatigue strength and stress-corrosion cracking resistance to chloride ions. PowderRange 625 has excellent weldability in laser and electron-beam additive manufacturing processes. Parts built from PowderRange® 625 can be heat treated and material properties can be varied within a specified range. Parts can be finished by all conventional means, including but not limited to machining, EDM, shot-peening, grit-blast, vibratory polishing, and coatings in both as-built and in heat treated conditions.

Type Analysis

  • Carbon (Maximum) 0.10
  • Phosphorus (Maximum) 0.015
  • Silicon (Maximum) 0.50
  • Nickel (Nominal) Balance
  • Titanium (Nominal) 0.40
  • Manganese (Maximum) 0.50
  • Sulfur (Maximum) 0.015
  • Chromium (Nominal) 20.00-23.00
  • Cobalt (Nominal) 1.00
  • Molybdenum (Nominal) 8.00-10.00
  • Iron (Maximum) 5.00
  • Aluminum (Maximum) 0.40
  • Nitrogen (Maximum) 0.020
  • Oxygen (Maximum) 0.030
  • Niobium (Nominal) 3.15-4.15