22Cr-13Ni-5Mn Stainless

UNS S20910

Composition (Nominal)
0.06 C, 4.00/6.00 Mn, 0.040 P, 0.030 S, 1.00 Si, 20.50/23.50 Cr, 11.50/13.50 Ni, 1.50/3.00 Mo, 0.10/0.30 Cb, 0.10/0.30 V, 0.20/0.40 N, Bal. Fe

Nitrogen-strengthened, austenitic stainless alloy, superior in corrosion resistance to Type 316, with twice the yield strength. Resists chloride pitting. BioDur 22Cr-13Ni-5Mn Stainless electroslag remelted (ESR) material has been used in medical implant devices.

Specifications: AMS 5764, AMS 5861, ASTM A240 (Grade XM-19), ASTM A276 (Grade XM-19), ASTM A412 (Grade XM-19), ASTM A479 (Grade XM-19), ASTM A580 (Grade XM-19), ASTM F1314

Carpenter Technology Corporation Carpenter Technology Corporation

Carpenter Technology Corporation (NYSE: CRS) is a recognized leader in high-performance specialty alloy-based materials and process solutions for critical applications in the aerospace, defense, transportation, energy, industrial, medical, and consumer electronics markets.

Learn More »