304/304L Stainless

UNS S30400/S30403

Composition (Nominal)
0.08 C, 2.00 Mn, 0.045 P, 0.030 S, 1.00 Si, 18.00/20.00 Cr, 8.00/10.50 Ni, Bal. Fe

304 stainless is the most widely used chromium-nickel austenitic stainless steel. It is nonmagnetic in the annealed condition and becomes slightly magnetic when cold worked. It has excellent fabricability and weldability characteristics. Nonhardenable by heat treating.

304L Stainless

Composition (Nominal)
0.03C, 2.00 Mn, 0.045 P, 0.03 S, 1.00 Si, 18.00/20.00 Cr, 8.00/12.00 Ni, Bal. Fe
Low-carbon content minimizes problem of carbide precipitation during welding and has permitted this alloy’s use in corrosive service in the as-welded condition.

Specifications: AMS 5639, AMS 5647, AMS 5697, ASTM A182, ASTM A193, ASTM A276, ASTM A314, ASTM A320, ASTM A479, MIL-S-862, QQ-S-763, QQS-W-423