310 Stainless

UNS S31000 | UNS 31008
Composition (Nominal)
0.25 C (except carbon reduced to 0.08% max. in Type 310S), 2.00 Mn, 0.045 P, 0.030 S, 1.50 Si, 24.00/26.00 Cr, 19.00/22.00 Ni, Bal. Fe

Both are austenitic chromium-nickel stainless steels having excellent oxidation resistance superior to Type 309. Resist temperatures up to 2100°F (1149°C) in continuous service, and provide good resistance to carburizing and reducing environments.

Specifications: ASTM A182, ASTM A276, ASTM A314, ASTM A479, ASTM A580, QQ-S-763