BioDur® 108 Alloy

UNS S29108

Weight Percent
0.08 C max., 23.00 Mn, 0.75 Si max., 0.03 P max., 0.01 S max., 21.00 Cr, 0.30 Ni max., 0.70 Mo, 0.25 Cu max., 0.97 N, Bal. Fe

BioDur 108 alloy is an essentially nickel-free austenitic stainless alloy with high nitrogen content to maintain its austenitic structure. The alloy's tensile and fatigue strength are superior to that of Type 316L (ASTM F138), 22Cr-13Ni-5Mn (ASTM F1314) and 734 alloy. Its pitting and crevice corrosion resistance is superior to Type 316L and equivalent to 22Cr-13Ni-5Mn and 734 alloy. Nonmagnetic and essentially free of ferrite phase.

Specifications: AMS 2630, ASTM F2229

Carpenter Technology Corporation Carpenter Technology Corporation

Carpenter Technology Corporation (NYSE: CRS) is a recognized leader in high-performance specialty alloy-based materials and process solutions for critical applications in the aerospace, defense, transportation, energy, industrial, medical, and consumer electronics markets.

Learn More »