BioDur® CCM Plus® Alloy

Composition (Nominal)
0.20/0.30 C, 26.00/30.00 Cr, 5.00/7.00 Mo, 0.15/0.20 N, Bal. Co

High carbon version of CarTech CCM® alloy produced by CarTech's Micro-Melt® powder metallurgy process. Vacuum induction melted, powder metal, non-magnetic, cobalt-chromium-molybdenum alloy exhibiting high strength, corrosion resistance, and wear resistance. Meets the requirements of ASTM F799, ASTM F1537, ISO 5832-4 and ISO 5832-12. This alloy is equivalent to ASTM F 1537 Alloy #2. Has been used in surgical implant devices.

Specifications: ASTM F1537, ASTM F75, ASTM F799, BS 7252, ISO 5832-12, ISO 5832-4