Chrome Core® 13-FM Alloy

U.S. Patent No. 5,769,974
Composition (Nominal)
0.03 C, 0.20/0.70 (13) - 0.50/1.20 (13-FM) Mn, 0.03 P, 0.03 (13) - 0.20/0.40 (13-FM) S, 0.70/1.80 Si, 12.50/13.50 Cr, 0.20/0.50 Mo, Bal. Fe

A family of controlled chemistry, ferritic chromium-iron alloys which should be considered for use in magnetic components where corrosion resistance superior to that of pure iron, low carbon steel and silicon-iron alloys is desired without the substantial decrease in saturation induction associated with the 18% Cr ferritic stainless steels. Applications could include electromechanical devices requiring some degree of corrosion resistance. Each chrome level is available in both a standard and a free-machining grade.
Carpenter Technology Corporation Carpenter Technology Corporation

Carpenter Technology Corporation (NYSE: CRS) is a recognized leader in high-performance specialty alloy-based materials and process solutions for critical applications in the aerospace, defense, transportation, energy, industrial, medical, and consumer electronics markets.

Learn More »