Composition (Nominal)
1.90 C, 0.35 Mn, 0.60 Si, 20.00 Cr, 0.65 W, 1.00 Mo, 4.00 V, Balance Fe

The unique combination of wear resistance, toughness, polishability and corrosion resistance makes CTS 204P an excellent candidate material for pelletizer, granulator and high-performance industrial and custom knives as well as food processing equipment. This alloy is now available in Strip product form.