CTS® XHP Alloy

(Composition (Nominal):)
1.60 C, 0.50 Mn, 0.40 Si, 16.00 Cr, 0.35 Ni, 0.80 Mo, 0.45 V, Bal. Fe

Air hardening, high carbon, high chromium, corrosion resistant alloy which can be described as either a high hardness Type 440C stainless steel or a corrosion resistant D2 tool steel. Possesses corrosion resistance equivalent to Type 440C stainless but can attain a maximum hardness of 64 HRC, approaching that of D2 tool steel. Now available in strip product form.

This proprietary alloy is in the CTS family of alloys that offer superior edge retention and surface finish, an ability to be machined to a fine edge, and consistent heat-treatability from lot to lot. Consider CTS alloys for many blade applications including commercial food processing, paper processing, textile, packaging, recycling/refuse, kitchen knives, hand tools, scissors/shears, shaving razors, sport/hunting knives, ice skates, military/defense, law enforcement, salon blades and various surgical/medical applications.

Carpenter Technology Corporation Carpenter Technology Corporation

Carpenter Technology Corporation (NYSE: CRS) is a recognized leader in high-performance specialty alloy-based materials and process solutions for critical applications in the aerospace, defense, transportation, energy, industrial, medical, and consumer electronics markets.

Learn More »