Custom 465® Stainless

UNS S46500

Composition (Nominal)
0.004 C, 11.70 Cr, 11.00 Ni, 1.00 Mo, 1.6 Ti, Bal Fe

Custom 465® stainless is a premium quality, high strength, age-hardening stainless alloy designed for improved notch tensile strength, fracture toughness and fabricability. This alloy has excellent resistance to stress corrosion cracking. Stress Corrosion cracking resistance of this alloy in the H 1000 condition is comparable to 13-8 stainless in the H 1050 condition.

General corrosion resistance similar to Type 304 stainless steel. Stress corrosion cracking resistance equal to 13-8 stainless. Strength superior to Custom 455® stainless.
Notched tensile strength superior to Custom 455. Fracture toughness equal to 13-8 stainless but at a higher strength and superior to Custom 455.

Has been used in medical instruments, small turbine engine shafts, sporting equipment and hand guns. Potential Applications include fasteners, aircraft actuators, upgrade 13-8 stainless and Custom 455 stainless components.

Specifications: AMS 5936, ASTM A564, ASTM A693, ASTM F899, MMPDS-01