Custom Flo 302HQ Stainless

UNS S30430
Composition (Nominal)
0.08 C, 2.00 Mn, 0.045 P, 0.03 S, 1.00 Si, 17.00/19.00 Cr, 8.00/10.00 Ni, 3.00/4.00 Cu, Bal. Fe

Slow work-hardening, austenitic stainless steel. Has been used for severe cold-heading applications such as nuts and recessed headed fasteners. Resistant to atmospheric corrosion and a wide variety of inorganic chemicals. Nonhardenable by heat-treating.

Specifications: ASTM A276, ASTM A493, ASTM F593