Composition (Nominal)
0.02 C, 0.50 Mn, 0.30 Si, 77.00 Ni, 2.5 Cr, 4.75 Cu, Bal. Fe

A high-permeability, soft magnetic alloy which has been used for certain magnetic shielding applications and having slightly improved cold-formability as compared to HyMu "80"® alloy.