Invar 36® Alloy

UNS K93601 | UNS K93603
Composition (Nominal):
0.02 C, 0.35 Mn, 0.20 Si, 36.00 Ni, Bal. Fe

A 36% nickel-iron alloy with a rate of thermal expansion approximately one-tenth that of carbon steel at temperatures up to 400°F (204°C). Has been used in applications such as radio and electronic devices where dimensional changes due to temperature must be minimal, as well as in support and structural members in precision optical laser mechanical measuring and positioning devices and for thermostat metals.

Specifications: ASTM B753 Alloy T36
CarTech Invar "36" alloy meets the requirements of specification ASTM B753 Alloy T36.
Carpenter Technology Corporation Carpenter Technology Corporation

Carpenter Technology Corporation (NYSE: CRS) is a recognized leader in high-performance specialty alloy-based materials and process solutions for critical applications in the aerospace, defense, transportation, energy, industrial, medical, and consumer electronics markets.

Learn More »