Composition (Nominal)
0.05/0.15 C, 1.00/2.00 Mn, 0.040 Si, 0.030 P, 0.3 S, 19.00/21.00 Cr, 9.00/11.00 Ni, 14.00/16.00 W, 3.00 Fe, Bal. Co

A nonmagnetic solid-solution strengthened cobalt base alloy that has good oxidation-corrosion resistance as well as high strength at elevated temperatures. Has been used for gas turbine rotors, nozzle diaphragm valves, springs, etc.

Specifications: AMS 5537, AMS 5796, AMS 5759F, ASTM F90, ISO 5832-5