M2 High Speed Steel

UNS T11302 | AISI Type M2
Composition (Nominal)
0.82 C, 0.30 Mn, 0.25 Si, 4.25 Cr, 5.00 Mo, 6.25 W, 1.80 V, Bal. Fe

Fine-grained molybdenum/tungsten high-speed steel which machines more easily than conventional 18-4-1 alloys, and is relatively lower in cost. Has been used for tools such as lathes, planers, drills, broaches, gear cutters, milling cutters.

Specifications: ASTM A600, QQ-T-590