Micro-Melt® M4 Alloy

UNS T11304 | AISI Type M4

Composition (Nominal)
1.35 C, 0.30 Mn, 0.30 Si, 0.06 S, 4.50 Cr, 4.50 Mo, 4.00 V, 5.50 W, Bal. Fe

A molybdenum/tungsten-bearing high-speed tool steel with high carbon and vanadium contents. This grade provides very high wear resistance along with high strength. It is manufactured using powder metallurgy processing techniques, and hot worked into various mill forms.