V-57 Alloy

AISI 663

Composition (Nominal)
0.08 C, 0.35 Mn, 0.50 Si, 0.015 P, 0.015 S, 13.50/16.00 Cr, 25.50/28.50 Ni, 1.00/1.50 Mo, 2.70/3.20 Ti, 0.50 V, 0.10/0.35 Al, 0.005/0.012 B, Bal. Fe

Iron-base austenitic, precipitation-hardening alloy for parts requiring high strength and good corrosion resistance at operating temperatures to 1400°F (760°C).