X-750 Alloy

UNS N07750 | AISI 688
Composition (Nominal)
0.08 C, 0.30 Mn, 0.50 Si, 0.010 S, 14.0/17.0 Cr, 70.00 Ni and Co, 2.25/2.70 Ti, 0.40/1.00 Al, 0.70/1.20 Cb and Ta, 0.05 Cu, 5.0/9.0 Fe

Precipitation-hardening alloy, highly resistant to chemical corrosion and oxidation. Has been used as high-temperature structural members for jet engine parts, heat-treating fixtures, forming tools.

Specifications: AMS 5667, AMS 5669, AMS 5671, AMS 5668, AMS 5670, MIL-N-8550 Condition E