410

UNS #S41000

410 stainless is the basic hardenable martensitic stainless steel suitable for highly stressed parts where corrosion resistance, good strength, and ductility are needed. This alloy can be used up to 1200ºF (649ºC) where resistance to scaling and oxidation is required.

Type Analysis

  • Carbon (Maximum) 0.15
  • Phosphorus (Maximum) 0.04
  • Silicon (Maximum) 1
  • Manganese (Maximum) 1
  • Sulfur (Maximum) 0.03
  • Chromium (Nominal) 11.50- 13.50
  • Iron (Nominal) Balance

Applicable Specifications

  • AMS 5613
  • ASTM A479
  • ASTM A580
  • QQ-S-763
  • ASTM A276
  • ASTM A493
  • ASTM F899

Bar

Flats

Rounds

Square

Billet

Strip

Wire

Rod