A-21®

UNS #S41429

A-21® stainless carburizing steel for wear-resistant applications that require excellent corrosion resistance, high strength, and good toughness, as well as applications that require excellent edge retention, high hardness, and stainless properties. An advanced martensitic stainless steel, it can be used in the carburized, nitrided, and normalized & tempered conditions. Unlike any other alloy, A-21® develops a deep, hard, stainless case and a strong, tough, ductile core after a streamlined carburizing process. It is also weldable and hardenable to very large section sizes (> 20) and supplied as annealed, 302 HB, max.

Type Analysis

Applicable Specifications

Bar

Flats

Hollow Bar

Rectangles

Rounds

Square

Billet

Plate

Strip

Coil

Sheet

Wire

Rod

RELATED RESOURCES

Browse our growing library of resources including case studies, product brochures, technical data sheets, product selection guides and more.