Biodur® 316LS

UNS #S31673

Biodur® 316LS stainless steel is an electro-slag remelted (ESR) or vacuum arc remelted (VAR), low carbon, high nickel and molybdenum version of 316 stainless. The secondary premium melting step (ESR or VAR) imparts improved cleanliness with chemistry modifications designed to maximize the corrosion resistance of this alloy and provide a ferrite free microstructure. The alloy is nonmagnetic even after severe cold forming operations and meets the requirements of ASTM F138, ASTM F139 and ISO 5832-1.

Type Analysis

  • Carbon (Maximum) 0.03
  • Phosphorus (Maximum) 0.025
  • Silicon (Maximum) 0.75
  • Nickel (Nominal) 13.00-15.00
  • Manganese (Maximum) 2
  • Sulfur (Maximum) 0.01
  • Chromium (Nominal) 17.00-19.00
  • Cobalt (Nominal) 0.1
  • Molybdenum (Nominal) 2.25-3.00
  • Iron (Nominal) Balance
  • Copper (Nominal) 0.5
  • Nitrogen (Nominal) 0.1

Applicable Specifications

  • ASTM F138
  • ISO 5832-1 Composition D
  • ASTM F139

Bar

Flats

Hexagons

Rounds

Square

Strip

Sheet

Wire

RELATED RESOURCES

Browse our growing library of resources including case studies, product brochures, technical data sheets, product selection guides and more.