C-276 is a nickel-molybdenum-chromium-tungsten alloy with excellent general corrosion resistance and good fabricability. The alloy should be considered for use in environments where resistance to hot contaminated mineral acids, organic and inorganic chloride-contaminated media, chlorine, formic and acetic acids, acetic anhydride, sea water, and brine solutions is desired. C-276 has resisted the formation of grain boundary precipitates in the weld heat-affected zone, making it a candidate for most chemical and petrochemical processing applications in the as-welded condition. The alloy has resisted both general and localized corrosion, including pitting, crevice corrosion, and stress corrosion cracking. C-276 is readily fabricated by welding, using methods similar to those utilized for nickel-based alloys.

Type Analysis

  • Carbon (Maximum) 0.02
  • Phosphorus (Maximum) 0.03
  • Silicon (Maximum) 0.08
  • Nickel (Nominal) Balance
  • Tungsten (Nominal) 3.00-4.50
  • Manganese (Maximum) 1
  • Sulfur (Maximum) 0.03
  • Chromium (Nominal) 14.50-16.50
  • Molybdenum (Nominal) 15.00-17.00
  • Iron (Nominal) 4.00-7.00
  • Vanadium (Maximum) 0.35
  • Cobalt (Maximum) 2.5

Downloads

Request a Quote

Applicable Specifications

  • ASME SB574
  • ASTM B574
  • ASME SB575
  • ASTM B575

Bar

Rounds

Strip

Wire